Explore and Study on Well Cementing Anti-Water-Channeling Self-Healing Agent
-
摘要: 针对固井后环空窜流遇水问题,笔者开发了防水窜自愈合剂。该防水窜自愈合剂为核壳结构,以高吸水树脂作为核心材料,吸水倍数从尺寸为100 μm开始呈指数增长,30 s内140目的样品吸水量达1898倍,120 s后达到稳定值,约2200倍;120目时吸水量在30 s也可达到892倍左右,120 s达到稳定值约1950倍。通过外部包裹后,其在水中可达到90℃下3 h不吸水的能力。在水泥水化后外壳破坏,其具有吸水自愈合能力。岩心实验表明,90℃下压差为2 MPa条件下防水窜自愈合剂40 min左右可完成裂缝封堵。含4%防水窜自愈合剂的常规密度水泥浆具有良好的流变性能,失水量可控,稠化时间线性正常,抗压强度较高,能够满足浅井固井水泥浆的需求。Abstract: An anti-water-channeling self-healing agent has been developed to deal with channeling in annular spaces after well cementing. This anti-water-channeling self-healing agent has a core-shell structure, it uses highly water absorbent resin as the core material and the size of the core (a sample passing 140 mesh screen) increases exponentially from original 100 μm to 1898 times of the original size in 30 s after absorbing water, and stabilizes at 2200 times of the original size in 120 s. Another 120-mesh sample absorbs water of 892 times of its original size in 30 s and stabilizes at 1950 times of the original size in 120 s. The core, after wrapped on its surface, does not absorb water for 3 h at 90℃. The anti-water-channeling self-healing agent can effectively plug fractures. When the cement is hydrated, the shell is broken and the anti-water-channeling self-healing agent then acquires water absorbency and self-healing ability. Core experiment showed that the anti-water-channeling self-healing agent can plug fractures in 40 min at 90℃and 2 MPa. Cement slurry test showed that normal density cement slurries containing 4% anti-water-channeling self-healing agent have good rheological property and controllable filtration rate, the thickening time of the cement slurries is linear and normal, and the set cement has high compressive strength, satisfying the needs of shallow well cementing.
-
Key words:
- Well cementing /
- Channeling in annular space /
- Cement slurry /
- Water channeling /
- Self-healing /
-
[1] 赵宝辉, 邹建龙, 刘爱萍, 等. 水泥基材料微裂缝自修复技术研究进展[J]. 钻井液与完井液, 2011, 28(S1):59-62.ZHAO Baohui, ZOU Jianlong, LIU Aiping, et al. Research progress on technology of micro-cracks self-healing with cement Matrix[J].Drilling Fluid & Completion Fluid, 2011, 28(S1):59-62. [2] 赵宝辉, 邹建龙, 石凌龙, 等. 油气井固井用自愈合剂研究与现场应用[C]//2016年固井技术研讨会论文集. 北京:石油工业出版社, 2016:444-451. ZHAO Baohui, ZOU Jianlong, SHI Linglong, et al. Research and application of self-healing cementing agent[C]//Proceedings of 2016 Cementing Technology Symposium. Beijing:Petroleum Industry Press, 2016:444-451. [3] 安少辉, 刘爱萍, 邹建龙, 等. 川渝地区复杂深井固井技术[J]. 钻井液与完井液, 2011, 28(S1):26-29.AN Shaohui, LIU Aiping, ZOU Jianlong, et al. Complex deep well cementing technology in SichuanChongqing region[J].Drilling Fluid & Completion Fluid, 2011, 28(S1):26-29. [4] 卢海川, 赵岳, 宋伟宾, 等. 新型固井用防水窜材料的研究与性能评价[J]. 钻井液与完井液, 2017, 34(4):75-79, 84. LU Haichuan, ZHAO Yue, SONG Weibin, et al.Study and evaluation of a new anti-water channeling material for well cementing[J].Drilling Fluid & Completion Fluid, 2017, 34(4):75-79, 84. [5] 马开华, 马兰荣, 陈武君. 高压油气井尾管回接固井新技术[J]. 石油钻采工艺, 2005, 27(3):22-23.MA Kaihua, MA Lanrong, CHEN Wujun.New technology for back-connection cementing of highpressure oil and gas wells[J].Oil Drilling & Production Technology, 2005, 27(3):22-23. [6] 张波, 管志川, 张琦, 等. 高压气井环空压力预测与控制措施[J]. 石油勘探与开发, 2015, 42(4):518-522.ZHANG Bo, GUAN Zhichuan, ZHANG Qi, et al. Predication of sustained annular pressure and pressure control measures of high pressure gas wells[J].Petroleum Exploration and Development, 2015, 42(4):518-522. [7] 李早元, 周超, 刘威, 等. 低温短候凝水泥浆体系室内研究[J]. 石油钻探技术, 2012, 40(2):46-50.LI Zaoyuan, ZHOU Chao, LIU Wei, et al. Laboratory study on the cement slurry system with short waiting on cementing time at low temperature[J].Petroleum Drilling Techniques, 2012, 40(2):46-50. [8] 赵宝辉, 邹建龙, 刘爱萍, 等. 自愈合水泥技术研究进展[C]//2012年固井技术研讨会论文集. 北京:石油工业出版社, 2012:35-43. ZHAO Baohui, ZOU Jianlong, LIU Aiping, et al. Research progress on self-healing cementing technology[C]//Proceedings of 2012 Cementing Technology Symposium.Beijing:Petroleum Industry Press, 2012:35-43. [9] 于永金, 靳建洲, 齐奉忠. 功能性固井工作液研究进展[J]. 钻井液与完井液, 2016, 33(4):1-7.YU Yongjin, JIN Jianzhou, QI Fengzhong.Progress of study on functional cementing fluids[J].Drilling Fluid & Completion Fluid, 2016, 33(4):1-7. [10] 宋有胜, 吴学升, 孙富全, 等. 自愈合水泥在长庆气井小间隙长水平井固井中的应用[J]. 石油化工应用, 2017, 36(2):23-28.SONG Yousheng, WU Xuesheng, SUN Fuquan, et al. Application of self-healing cement in long horizontal well cementing in Changqing gas well[J].Petrochemical Industry Application, 2017, 36(2):23-28. [11] 宋有胜, 邹建龙, 赵宝辉, 等. 高石梯-磨溪区块高压气井尾管固井技术[J]. 钻井液与完井液, 2017, 34(2):111-116.SONG Yousheng, ZOU Jianlong, ZHAO Baohui, et al. Liner cementing the high pressure gas wells in the block Gaoshiti-Moxi[J].Drilling Fluid & Completion Fluid, 2017, 34(2):111-116. [12] 田宝振, 李清洁, 覃毅, 等.塔中碎屑岩井自愈合水泥浆固井技术[J]. 钻井液与完井液, 2016, 33(6):84-90.TIAN Baozhen, LI Qingjie, QIN Yi, et al.Cementing wells penetrating clastic rocks with self-healing cement in block Tazhong[J].Drilling Fluid & Completion Fluid, 2016, 33(6):84-90. [13] 郭丽梅, 耿国伟, 霍丙夏. 新型自愈合水泥研制[J]. 钻井液与完井液, 2014, 31(6):55-57.GUO Limei, GENG Guowei, HUO Bingxia. Research of novel self-healing cement[J].Drilling Fluid & Completion Fluid, 2014, 31(6):55-57. [14] 步玉环, 柳华杰, 赵乐天, 等. 固井水泥石微裂缝遇水自封堵机理分析及验证[C]//2016年固井技术研讨会论文集. 北京:石油工业出版社, 2016:31-41. BU Yuhuan, LIU Huajie, ZHAO Letian, et al. Mechanism analysis and verification of micro-cracks self-blocking with water in cement set[C]//Proceedings of 2016 Cementing Technology Symposium. Beijing:Petroleum Industry Press, 2016:31-41.
点击查看大图
计量
- 文章访问数: 828
- HTML全文浏览量: 228
- PDF下载量: 156
- 被引次数: 0