射孔完井工况下固井水泥环破坏研究进展

李进 龚宁 李早元 韩耀图 袁伟伟

李进, 龚宁, 李早元, 韩耀图, 袁伟伟. 射孔完井工况下固井水泥环破坏研究进展[J]. 钻井液与完井液, 2016, 33(6): 10-16. doi: 10.3969/j.issn.1001-5620.2016.06.002
引用本文: 李进, 龚宁, 李早元, 韩耀图, 袁伟伟. 射孔完井工况下固井水泥环破坏研究进展[J]. 钻井液与完井液, 2016, 33(6): 10-16. doi: 10.3969/j.issn.1001-5620.2016.06.002
LI Jin, GONG Ning, LI Zaoyuan, HAN Yaotu, YUAN Weiwei. Progress in Studying Cement Sheath Failure in Perforated Wells[J]. DRILLING FLUID & COMPLETION FLUID, 2016, 33(6): 10-16. doi: 10.3969/j.issn.1001-5620.2016.06.002
Citation: LI Jin, GONG Ning, LI Zaoyuan, HAN Yaotu, YUAN Weiwei. Progress in Studying Cement Sheath Failure in Perforated Wells[J]. DRILLING FLUID & COMPLETION FLUID, 2016, 33(6): 10-16. doi: 10.3969/j.issn.1001-5620.2016.06.002

射孔完井工况下固井水泥环破坏研究进展

doi: 10.3969/j.issn.1001-5620.2016.06.002
基金项目: 

国家十三五重大科技专项“渤海油田高效钻完井及配套技术示范工程下属子课题:复杂油层精细射孔与评价工艺技术研究及应用”(2016ZX05009002-005);国家自然科学基金项目“基于多相渗流理论的环空气窜机理及应用基础研究”(51574203)

详细信息
    作者简介:

    李进,1988年生,工程师,硕士,主要从事油气井完井射孔、防砂及固完井技术研究。电话(022)66501136;E-mail:lijin201220011@126.com。

    通讯作者:

    李早元,电话13982045007

  • 中图分类号: TE256.9

Progress in Studying Cement Sheath Failure in Perforated Wells

  • 摘要: 射孔完井作为国内外应用最为广泛的完井方式,对油气井增产有着非常重要的意义。随着射孔完井的不断推广,射孔后水泥环层间封隔完整性越来越受到重视,尤其是薄差油气层,而现有研究主要集中于射孔后套管损害及强度影响,对射孔完井工况下水泥环破坏涉及较少。为了更好地促进射孔后水泥环完整性的研究与发展,结合油气井射孔威力大、时间短、温度高、破坏性强等特点,分析指出了射孔完井工况下固井水泥环破坏研究难点主要集中于室内射孔模拟实验难、射孔后水泥环完整性破坏程度难确定、实际工况下水泥环抗冲击破坏能力难确定以及射孔参数影响不清楚等方面,综述了国内外射孔模拟实验、射孔水泥环完整性、水泥环抗冲击韧性、射孔作业参数影响的研究现状,探讨了目前研究存在的不足。提出了以自修复水泥、水泥浆及水泥石性能设计、优化射孔参数、井下水泥环动态破坏预测技术为核心的技术对策与趋势。

     

  • [1] 刘合, 王峰, 王毓才, 等. 现代油气井射孔技术发展现状与展望[J]. 石油勘探与开发, 2014, 41(6):731-737.

    LIU He, WANG Feng, WANG Yucai, et al. Oil well perforation technology:status and prospects[J]. Petroleum Exploration and Development, 2014, 41(6):731-737.
    [2] 袁吉诚. 中国射孔技术的研究与发展[J]. 测井技术, 2002, 26(5):421-425.

    YUAN Jicheng. Advances of the perforating technology in China[J]. Well Logging Technology, 2002, 26(5):421-425.
    [3] BAKKER E, VEEKEN K, BEHRMANN L, et al. Technology of dynamic negative pressure perforation[J]. World Well Logging Technology, 2004, 19(5):48-60.
    [4] 万仁傅. 现代完井工程[M]. 北京:石油工业出版社, 2000. WAN Renfu. Modern completion project[M].Beijing:Petroleum Industry Press, 2000.
    [5] 王伯军, 温玉焕. 均匀载荷下高密度射孔参数对套管抗挤强度的影响[J]. 石油钻探技术, 2008, 36(1):50-52.

    WANG Baijun, WEN Yuhuan. Effects of high-density perforation parameters on collapsing strength under uniform loading[J]. Petroleum Drilling Techniques, 2008, 36(1):50-52.
    [6] 郭小阳, 杨远光, 李早元, 等. 提高复杂井固井质量的关键因素探讨[J]. 钻井液与完井液, 2007(S1):53-58. GUO Xiaoyang, YANG Yuanguang, LI Zaoyuan, et al. Key factors to improve the quality of complex well cementing[J]. Drilling Fluid & Completion Fluid, 2007

    (S1):53-58.
    [7] 汪艳. 内压对套管射孔强度影响的有限元分析[J]. 机械, 2011, 28(5):19-22.

    WANG Yan. Finite element analysis of the effect of internal pressure on perforated casing strength[J]. Machinery, 2011, 28(5):19-22.
    [8] 王祥林, 王允良, 王立平, 等. 射孔对水泥环损伤的综合试验研究[J]. 地震工程与工程振动, 1994, 14(1):89-99.

    WANG Xianglin, WANG Yunliang, WANG Liping, et al. Synthetic experimental research on the damage to the circle during the hole shooting[J].Earthquake Engineering and Engineering Vibration, 1994, 14(1):89-99.
    [9] 王祥林, 王允良, 王立平, 等. 射孔对水泥环损伤的综合试验研究[J]. 地震工程与工程振动, 1994, 14(1):89-99.

    WANG Xianglin, WANG Yunliang, WANG Liping, et al. Synthetic experimental research on the damage to the circle during the hole shooting[J]. Earth Quake Engineering and Engineering Vibration, 1994, 14(1):89-99.
    [10] 王祥林, 黄义春, 牛丽君, 等. 固井工程中的抗窜研究[J]. 石油学报, 1999, 20(4):88-92.

    WANG Xianglin, HUANG Yichun, NIU Lijun, et al. A research on preventing and resisting the oil permeation in well cementation[J]. Acta Petroleisinica, 1999, 20(4):88-92.
    [11] 莫继春, 李杨, 卢东红, 等. 霍布金森水泥石动态力学性能与射孔验窜试验装置[J]. 钻井液与完井液, 2004, 21(6):8-11.

    MO Jichun, LI Yang, LU Donghong, et al. Instruments for cement stone dynamics properties and perforating channeling testing based on hopkinon spill pressure[J]. Drilling Fluid & Completion Fluid, 2004, 21(6):8-11.
    [12] 穆海朋, 步玉环, 姜林甫, 等. 固井纤维水泥射孔实验研究[J]. 石油钻采工艺, 2007, 29(4):28-31.

    MU Haipeng, BU Yuhuan, JIANG Linfu. Perforation experiment of fiber cement for cementing[J].Oil Drilling & Produnction Technology, 2007, 29(4):28-31.
    [13] SAUCLER R J, LANDS J F. A laboratory study of perforations in stressed formation rocks[C].SPE 6758, 1978.
    [14] GENE D. Effects of formation compressive strength on perforator performance[C]. Spring Meeting of the Southern District, API Division of Production, March 1962.
    [15] ZINKHAM R E, GOODWIN R J. Burst resistance of pipe cemented into the earth[C]. SPE 291, 1962.
    [16] THIERCELIN M J. A soil mechanics approach to predict cement sheath behavior[C].SPE 47375, 1998.
    [17] BOSMA M. Design approach to sealant selection for the life of the well[C].SPE 56535, 1999.
    [18] MUELLER D T. Characterizing casing-cement-formation interactions under stess conditons:impact on long-term zonal isolation[C]. SPE 90450, 2004.
    [19] JEREMIE SAINT MARC, ANDRE GARNIER.Intinal state of stress:the key to achieving long-term cementsheath integrity[C]. SPE 116651, 2008.
    [20] 李军, 陈勉, 柳贡慧, 等. 套管、水泥环及井壁围岩组合体的弹塑性分析[J]. 石油学报, 2005, 26(6):99-103.

    LI Jun, CHEN Mian, LIU Gonghui, et al. Casing, cement loop and well rock elastic-plastic analysis of combination[J].Acta Petroleisinica, 2005, 26(6):99-103.
    [21] 刘健. 油气井水泥石力学行为本构方程与完整性评价模型研究[D]. 西南石油大学油气井工程, 2013. LIU Jian. Research on constitutive equation and integrity evaluation model of oil and gas wells debris mechanical behavior[D].Southwest Petroleum University, 2013.
    [22] 郭小阳, 程小伟, 张春梅, 等. 油气井水泥生产与应用[M]. 北京:石油工业出版社, 2013. GUO Xiaoyang, CHENG Xiaowei, ZHANG Chunmei, et al. Production and application of oil and gas well cement[M]. Beijing:Petroleum Industry Press, 2013.
    [23] ALTUNA G, JUAN E. Variation of the mechanical properties for cementing slurries with different compositions[C]. SPE 69616, 2001.
    [24] 华苏东, 姚晓. 复合纤维提高油井水泥石韧性的研究[J]. 钻井液与完井液, 2007, 24(4):40-42.

    HUA Sudong, YAO Xiao. Composite fiber improves the toughness of oil-well set cement[J]. Drilling Fluid & Completion Fluid, 2007, 24(4):40-42.
    [25] YAO X, HUA S D. Design of a novel composite agent for improving the toughness of oilwell cement sheath[C]. SPE 106010, 2007.
    [26] 朱磊, 耿亚楠, 许明标, 等. 适合小井眼固井的韧性水泥浆体系室内研究[J]. 石油天然气学报(江汉石油学院学报), 2014, 36(9):106-112. ZHU Lei, GEN Yanan, XU Mingbiao, et al. Laboratory research of malleable cement slurry system suitable for slim-hole cementing[J]. Journal of Oil and Gas Technology, 2014, 36(9):106-112.
    [27] 王文斌, 马海忠, 魏周胜, 等. 抗冲击韧性水泥浆体系室内研究[J]. 钻井液与完井液, 2004, 21(1):36-39.

    WANG Wenbin, MA Haizhong, WEI Zhousheng, et al. Laboratory study on impact resistance toughness cement slurry system[J]. Drilling Fluid & Completion Fluid, 2004, 21(1):36-39.
    [28] GODFREY W K, METHVEN N E. Casing damage caused by jet perforating[C].SPE 3043, 1970.
    [29] GODFREY W K. Effect of jet perforating on bond strength of cement[J]. Journal of Petroleum Technology, 1968:1301-1314.
    [30] KING G E. The effect of high-density perforating on the mechanical crush resistance of casing[C].SPE 18843, 1989.
    [31] 王正国, 陈风波. 射孔参数对套管强度影响有限元分析[J]. 国外测井技术, 2007, 22(6):37-39.

    WANG Zhengguo, CHEN Fengbo. Finite element analysis of effect of perforation parameters on casing strength[J].World Well Logging Technology,2007,2(26):37-39.
    [32] KLOTZ J A, KRUEGER, PYE D S. Effect of perforation damage on well productivity[C].SPE 4654, 1974.
    [33] 李海涛, 王永清. 裂缝性油藏射孔参数对油井产能的影响研究[J]. 西南石油学院学报, 2006, 28(3):70-73.

    LI Haitao, WANG Yongqing. Study on the effect of perforating parameters upon well productivity in natural fracture reservoirs[J].Journal of Southwest Petroleum Institute, 2006, 28(3):70-73.
    [34] 徐贵春, 徐苏欣, 唐海军, 等. 水平井射孔参数优化研究与应用[J]. 复杂油气藏, 2009, 4(2):61-66.

    XU Guichun, XU Suxing, TANG Haijun, et al. Optimization research and application of perforating parameters of horizontal well[J]. Complex Hydrocarbon Reservoirs, 2009, 4(2):61-66.
  • 加载中
计量
  • 文章访问数:  1307
  • HTML全文浏览量:  311
  • PDF下载量:  624
  • 被引次数: 0
出版历程
  • 收稿日期:  2016-09-12
  • 刊出日期:  2016-11-30

目录

    /

    返回文章
    返回

    欢迎订阅

    2025年《钻井液与完井液》,邮发代号为:18-423,编辑部不受理订阅业务。