海上油气井环空带压高强度环氧基封堵剂的研制及封堵机理

苏延辉 李志臻 胡秉磊 张云飞 桂鹏 姜雨省 耿学礼

苏延辉,李志臻,胡秉磊,等. 海上油气井环空带压高强度环氧基封堵剂的研制及封堵机理[J]. 钻井液与完井液,2026,43(2):280-288 doi: 10.12358/j.issn.1001-5620.2026.02.017
引用本文: 苏延辉,李志臻,胡秉磊,等. 海上油气井环空带压高强度环氧基封堵剂的研制及封堵机理[J]. 钻井液与完井液,2026,43(2):280-288 doi: 10.12358/j.issn.1001-5620.2026.02.017
SU Yanhui, LI Zhizhen, HU Binglei, et al.Development and plugging mechanism of high strength epoxy resin-based plugging agent used in offshore oil and gas wells with sustained annular pressure[J]. Drilling Fluid & Completion Fluid,2026, 43(2):280-288 doi: 10.12358/j.issn.1001-5620.2026.02.017
Citation: SU Yanhui, LI Zhizhen, HU Binglei, et al.Development and plugging mechanism of high strength epoxy resin-based plugging agent used in offshore oil and gas wells with sustained annular pressure[J]. Drilling Fluid & Completion Fluid,2026, 43(2):280-288 doi: 10.12358/j.issn.1001-5620.2026.02.017

海上油气井环空带压高强度环氧基封堵剂的研制及封堵机理

doi: 10.12358/j.issn.1001-5620.2026.02.017
基金项目: 中海油能源发展股份有限公司井筒完整性重大专项子课题 “套管间环空带压井不动管柱治理技术研究”(HFKJ-ZX-GJ-2023-06-03)。
详细信息
    作者简介:

    苏延辉,高级工程师,博士,1982年生,主要从事钻采化学品的研发和技术应用工作。E-mail:suyh@cnooc.com.cn

    通讯作者:

    李志臻,高级工程师,1987年生。E-mail:lizhzh9@cnooc.com.cn

  • 中图分类号: TE257

Development and Plugging Mechanism of High Strength Epoxy Resin-Based Plugging Agent Used in Offshore Oil and Gas Wells with Sustained Annular Pressure

  • 摘要: 海上油气井的环空压力积聚问题在高温高压下尤为突出,易引发泄漏、腐蚀及井筒结构失效,严重威胁作业安全与井筒完整性。针对传统水泥和树脂类封堵材料在流动性、固化可控性及力学性能方面存在的局限性,研制了一种适用于不动管柱条件下施工的新型高强度环氧基封堵剂。该材料由35%~55%环氧树脂、5%超支化树脂、20%~30%稀释剂和10%~40%中温固化剂复配而成。基于室内实验评估了新型高强度环氧基封堵剂的流变学行为、力学性能、热稳定性和密封能力。结果表明,该封堵剂在25 ℃~65 ℃下具有良好的流动性(黏度为35~185 mPa·s),固化时间可控制在0.11~25 h之间,抗压强度达到31~63 MPa,20 ℃~100 ℃范围内胶结强度均大于11 MPa/8 cm;热稳定性优异(分解温度高达380 ℃),并在20 MPa气压下实现零渗透。该封堵剂兼具高强度、高耐温与良好密封性,具备在复杂海洋环境中应用的可行性,可为海上环空压力控制提供技术支撑。

     

  • 图  1  SF-F2树脂的合成示意图

    图  2  SF-F2型树脂的红外光谱图

    图  3  封堵剂的黏度随温度的变化

    图  4  封堵剂的黏度随稀释剂加量的变化(25 ℃)

    图  5  封堵剂的固化时间随固化剂加量的变化

    图  6  抗压强度随温度的变化

    图  7  封堵剂的胶结强度随温度的变化

    图  8  胶结强度测试实验后钢管内部的扫描电镜图

    图  9  封堵剂的热失重测试结果

    图  10  高强度树脂封堵剂在复杂井筒环境的高效封隔机制示意图

    表  1  不同固化剂加量和不同温度下封堵剂的固化时间

    T固化/
    不同固化剂加量下的固化时间/min
    25% 30% 35%
    40 614 493 350
    50 535 420 303
    70 526 413 286
    下载: 导出CSV
  • [1] 唐浩瑞, 吴小龙, 雷正, 等. 海上某气井环空带压安全管控研究[J]. 中国石油和化工标准与质量, 2024, 44(11): 72-74,77.

    TANG Haorui, WU Xiaolong, LEI Zheng, et al. Research on safety management and control of annular pressure buildup in an offshore gas well[J]. China Petroleum and Chemical Standard and Quality, 2024, 44(11): 72-74,77.
    [2] 王捷力, 董雪林, 高德利. 超深气井环空带压分析与控制研究[J]. 钻采工艺, 2024, 47(4): 65-73.

    WANG Jieli, DONG Xuelin, GAO Deli. Research on analysis and control of annular pressure in ultra-deep gas wells[J]. Drilling & Production Technology, 2024, 47(4): 65-73.
    [3] 李强, 武治强, 何英明, 等. 海上气井环空带压管理方案研究及应用[J]. 中国海上油气, 2019, 31(3): 140-146.

    LI Qiang, WU Zhiqiang, HE Yingming, et al. Research and application of management program for annular pressure in offshore gas wells[J]. China Offshore Oil and Gas, 2019, 31(3): 140-146.
    [4] 李建伍. 石油开采井下作业堵水技术分析[J]. 化工管理, 2017(25): 218.

    LI Jianwu. Analysis of water plugging technology for downhole operations in petroleum production[J]. Chemical Enterprise Management, 2017(25): 218.
    [5] 胡旭光, 刘贵义, 胡光辉. “带压钻孔+冷冻暂堵”组合工艺治理井口隐患[J]. 天然气技术与经济, 2020, 14(1): 53-56,63.

    HU Xuguang, LIU Guiyi, HU Guanghui. Drilling under pressure and frozen temporary plugging to remove hidden troubles at wellhead for complex gas wells[J]. Natural Gas Technology, 2020, 14(1): 53-56,63.
    [6] YANG J B, BAI Y R, SUN J S, et al. Curing kinetics and plugging mechanism of high strength curable resin plugging material[J]. Petroleum Science, 2024, 21(5): 3446-3463. doi: 10.1016/j.petsci.2024.04.016
    [7] YUAN J L, ZHAO X W, YE L. Structure and properties of urea-formaldehyde resin/polyurethane blend prepared via in-situ polymerization[J]. RSC Advances, 2015, 5(66): 53700-53707. doi: 10.1039/C5RA06029J
    [8] 赵林, 高申领, 陈渊, 等. 砂岩油藏聚合物堵塞机理及解堵方法研究[J]. 特种油气藏, 2022, 29(3): 156-161.

    ZHAO Lin, GAO Shenling, CHEN Yuan, et al. Study on polymer plugging mechanism and plug removal method in sandstone reservoirs[J]. Special Oil & Gas Reservoirs, 2022, 29(3): 156-161.
    [9] 魏安超, 刘书杰, 蒋东雷, 等. 裂缝性储层环氧树脂自降解堵漏剂的制备与评价[J]. 钻井液与完井液, 2023, 40(2): 163-168.

    WEI Anchao, LIU Shujie, JIANG Donglei, et al. Synthesis and evaluation of epoxy resin self-degradation plugging agent for fractured formation[J]. Drilling Fluid & Completion Fluid, 2023, 40(2): 163-168
    [10] ZHANG X F, PENG Z G, FENG Q, et al. Effect of CTBN and Nano-SiO2 modified epoxy resin powder on the mechanical properties of cement-based composites[J]. Journal of Building Engineering, 2024, 83: 108456. doi: 10.1016/j.jobe.2024.108456
    [11] GENEDY M, KANDIL U F, MATTEO E N, et al. A new polymer nanocomposite repair material for restoring wellbore seal integrity[J]. International Journal of Greenhouse Gas Control, 2017, 58: 290-298. doi: 10.1016/j.ijggc.2016.10.006
    [12] LIU W T, SUN Y D, MENG A N, et al. Experimental analysis of Nano-SiO2 modified waterborne epoxy resin on the properties and microstructure of cement-based grouting materials[J]. Energy, 2023, 268: 126669. doi: 10.1016/j.energy.2023.126669
    [13] 张鹏, 吴靖江, 张承实, 等. 纳米 SiO2 和混杂纤维增强环氧树脂水泥基修复材料的抗折性能和微观结构[J]. 硅酸盐通报, 2025, 44(3): 834-841.

    ZHANG Peng, WU Jingjiang, ZHANG Chengshi, et al. Flexural properties and microstructure of nano-SiO2 and hybrid fiber reinforced epoxy resin cement-based repair materials[J]. Bulletin of the Chinese Ceramic Society, 2025, 44(3): 834-841.
    [14] 周俊, 彭志刚, 董志明, 等. 超支化树脂的制备及其对环氧树脂封窜剂性能的影响[J]. 合成化学, 2025, 33(7): 487-494.

    ZHOU Jun, PENG Zhigang, DONG Zhiming, et al. Preparation of hyperbranched resin and its effect on the performance of epoxy resin sealing agent[J]. Chinese Journal of Synthetic Chemistry, 2025, 33(7): 487-494.
    [15] 王瑞, 陈神根, 徐金山, 等. 抗CO2腐蚀特种树脂水泥体系的构建及其性能评价[J]. 化学研究与应用, 2025, 37(2): 344-352.

    WANG Rui, CHEN Shengen, XU Jinshan, et al. Construction and performance evaluation of CO2 resistant special resin cement system[J]. Chemical Research and Application, 2025, 37(2): 344-352.
    [16] 罗黎敏. 用于油气井环空带压治理的聚合物凝胶体系研究[J]. 当代化工, 2023, 52(7): 1624-1627.

    LUO Limin. Study on polymer gel system for treatment of sustained casing pressure in oil and gas wells[J]. Contemporary Chemical Industry, 2023, 52(7): 1624-1627.
    [17] 李文哲, 付志, 张震, 等. 用于诱导微裂缝封堵的油基凝胶体系[J]. 钻井液与完井液, 2023, 40(4): 446-452,461.

    LI Wenzhe, FU Zhi, ZHANG Zhen, et al. Study and application of an oil-based gel fluid for sealing induced micro-fractures[J]. Drilling Fluid & Completion Fluid, 2023, 40(4): 446-452,461
    [18] 严鸿伟. 深水气井环空带压分析及防治措施研究[D]. 成都: 西南石油大学, 2019.

    YAN Hongwei. Analysis of annular pressure in deep water gas wells and prevention measures[D]. Chengdu: Southwest Petroleum University, 2019.
    [19] 吴艳辉, 代锐, 张磊, 等. 深水井筒海水聚合物钻井液水合物生成抑制与堵塞物处理方法[J]. 钻井液与完井液, 2023, 40(4): 415-422.

    WU Yanhui, DAI Rui, ZHANG Lei, et al. Study on methods of gas hydrate inhibition and blockage treatment using seawater polymer muds in deepwater well drilling[J]. Drilling Fluid & Completion Fluid, 2023, 40(4): 415-422
    [20] 刘浩亚. 治理环空带压的密封剂的研制与评价[J]. 钻井液与完井液, 2022, 39(3): 334-338.

    LIU Haoya. Development and evaluation of sealant for controlling annular pressure[J]. Drilling Fluid & Completion Fluid, 2022, 39(3): 334-338
    [21] 韩荣. 反应溶剂与催化剂适配实现高度耐腐蚀树脂高效降解[N]. 科技日报, 2023-03-11(006).

    HAN Rong. Reactive solvent and catalystenable efficient degradation of highly corrosion-resistant resins[N]. Science and Technology Daily, 2023-03-11(006).
  • 加载中
图(10) / 表(1)
计量
  • 文章访问数:  10
  • HTML全文浏览量:  2
  • PDF下载量:  2
  • 被引次数: 0
出版历程
  • 收稿日期:  2025-09-20
  • 修回日期:  2025-11-25
  • 刊出日期:  2026-04-08

目录

    /

    返回文章
    返回

    尊敬的作者、读者:

    您好!

    为更好地服务于广大作者和读者,提升期刊编辑部的办公效率和服务质量,本刊编辑部办公地点及联系电话已进行变更。

    新办公地址:天津经济技术开发区第二大街83号中国石油天津大厦A517房间

    新联系电话:022-65278734

                         022-25275527

    我们衷心希望广大作者和读者能够继续支持我们的工作,共同推动期刊的发展和进步。

    再次感谢您对期刊的关注和支持!